Failure Analysis of High Speed High Temperature PTFE Lip Seals for Engine Applications

PTFE lip seals can withstand temperatures of up to 260 °C, but in high-speed engine conditions they tend to fail early. And if it fails, oil leaks out, the machine is disabled and repair expenses mount up immediately.

Under such circumstances, a PTFE lip seal faces a challenging task. It has to retain oil in the engine as the shaft is rotating at high speeds and the temperature is rising. In times of heat and wear, even the strongest seal will fail.

Why PTFE Lip Seals Are Used in Engines

Rubber seals age fast under heat. They harden and crack when speeds rise. PTFE lip seals handle these limits far better. It is a durable, low friction plastic, which is not affected by Oil and most chemicals. This is why it is employed by engine manufacturers in the manufacture of crankshafts and gearboxes.

Unlike rubber, a plain PTFE lip will not pump oil back. Some designs add a spiral groove to fix this. Still, every PTFE lip seal can fail when the working conditions go beyond its limits.

Bronze PTFE Hydraulic Rod Seal Step Seal with NBR/FKM O-Ring

How High Speed and Heat Stress a PTFE Lip Seal

Fast shafts create friction at the sealing edge. Friction turns into heat. Studies on aero engine seals show that more speed means more heat and weaker sealing. Heat also thins the oil film. A thin film means more contact and faster wear.

More stress is caused by pressure and vibration. Soot and metal bits are also carried with the engine oil. These particles scratch the shaft and lip. Over time the PTFE lip seals lose contact pressure and begin to leak.

Common Failure Modes of PTFE Lip Seals

The same issues keep arising in the engineering field. Most common ones are shown below in the table.

Failure Mode Main Sign Likely Cause
Lip wear Thin or flat lip edge High speed and dry running
Shaft scoring Grooves on the shaft Hard dirt or rough shaft finish
Heat damage Glazed or discolored lip Too much friction heat
Cold flow Lip loses shape Constant high load
Leakage at the outer edge Oil near the housing Poor fit or bad installation

Excess Wear on the PTFE Lip Seal

Wear is the top failure in engines. Each turn of the shaft thins the lip a little. Less lip means less contact force, then oil slips past. Dry starts and weak oil films speed this up. Filled PTFE grades often last longer here.

Shaft Damage and PTFE Lip Seals

PTFE is soft compared with steel. A rough or scratched shaft cuts the lip fast. A narrow groove can create a leakage area. Many shafts require a very fine finish, with no spiral machining marks. A hardened surface also helps PTFE lip seals last longer.

Heat Damage and Cold Flow in a PTFE Lip Seal

PTFE handles heat well but under steady load it can slowly creep. This is called cold flow. Then the lip loses its shape and its grip on the shaft. Extra heat makes creep worse and glazed or dark lips are clear signs.

Poor Lubrication and Dry Running in PTFE Lip Seals

Engines face dry starts and low oil levels. Without oil the lip rubs bare metal. Then the temperature rises in seconds. With low friction, PTFE runs without the aid of a lubricant, whereas rubber does not. However, prolonged periods of dryness can cause the lip to become burnt. Clean and good oil flow can protect every PTFE lip seal.

Installation Errors That Harm PTFE Lip Seals

PTFE does not bounce back like rubber. A nick or fold during fitting is permanent. Sharp shaft edges and missing lead-in chamfers cause damage. Misaligned housings add uneven load. Always use fitting tools and clean parts. Check the lip direction before pressing in the PTFE lip seals.

Root Causes Behind PTFE Lip Seal Failure

There are some root causes that cause most failures. In knowing them, you will be able to solve the actual problem and not just replace the part.

Wrong material grade for the speed and temperature

Shaft finish that is too rough or too smooth

Shaft runout or housing misalignment

Dirty oil with soot or metal particles

Oil level or flow that is too low

Fitting damage from poor tools or methods

How to Run a Failure Analysis on PTFE Lip Seals

A clear process saves time and money. If a seal has a leak, then follow the steps below:

Record the RPM at failure and the oil temp at failure.

Take pictures prior to taking the seal off.

Check the oil for dirt and burning.

Examine the shaft finish and for grooves.

Inspect lip under magnifier for wear and glazing.

Compare the shape of the lip to a new seal.

Write the cause and change the design or process.

Lip Seal Failure Analysis

Ways to Prevent PTFE Lip Seal Failure

Prevention costs far less than repair. These habits keep a PTFE lip seal working longer in hard engine duty.

Pick a filled PTFE grade for high speed and heat

Keep the shaft hardness and finish within the seal maker's advice

Use clean oil and change it on time

Add a spiral groove design when back pumping is needed

Control shaft runout and alignment

Train fitters to use proper tools

Choosing the Right Material for PTFE Lip Seals

Fillers alter the properties of PTFE. They are each designed for a different use. Simply use the list below and follow the guidelines.

Bronze-filled PTFE: strong and good for heat transfer

Carbon-filled PTFE: low wear and good for dry running

Graphite filled PTFE: low friction against softer shafts

MoS2-filled PTFE: reduced friction and extended wear life.

Glass-filled PTFE: excellent wear performance and chemical resistance.

Virgin PTFE: pure and suitable for clean or food applications.

Always match the grade with the type of oil and shaft metal. A hard filler on a soft shaft can cause scoring. Test samples under real engine speed and heat when possible.

DMS Seals Solutions for PTFE Lip Seals

DMS Seals is a professional seal maker based in China. It started in 2008 with PTFE products. Today the team has 120 staff including 70 senior technicians. The factory area is over 10,000 sqm. DMS Seals is ISO 9001 and TS 16949 Certified.

It can be used in engine and hydraulic applications. You can choose from these products:

Oil seals in TC, TB, SC, DC and TCV types

Rotary seals for spinning shafts

Spring energized seals made for your application

Rod seals and piston seals in bronze or carbon filled PTFE

O rings in NBR, FKM, silicone, EPDM, HNBR and FFKM

DMS Seals also offers OEM and ODM services. Its labs test friction and tensile strength. Contact the team to discuss PTFE lip seals for your engine.

Conclusion

Failure in PTFE lip seals rarely has one cause. All contribute to the causes of heat, speed, shaft damage, poor oil and fitting errors. The true cause is revealed by careful failure analysis. Then the right grade, shaft finish and fitting method can stop repeat leaks. Small changes often bring big gains in seal life and engine uptime.

Need a sealing partner for demanding engines? Talk to DMS Seals today. Provide car speed, temperature and oil information. We will guide you to obtaining a good PTFE lip seal or a custom solution. Our engineers reply fast and also offer OEM and ODM support.

Send your inquiry and get a quick offer.

FAQs

How hot can the PTFE lip seal get?

Many designs are suitable for up to 260 °C; the actual limit is dependent on filler and oil. Please check the data sheet for your grade.

What causes lip seals to leak at high speed in the case of PTFE?

Lip contact force is diminished with heat and wear. Oil cannot be pumped back out of a plain lip, either. Leaks are more probable in the presence of rough shafts and dirty oil.

Is it possible for a PTFE lip seal to dry out?

It is more tolerant of short dry periods than rubber. The lip continues to burn when it is left alone for a long time. Maintain uninterrupted supply of oil to protect.

When does a PTFE lip seal fail?

Check for oil spots close to the shaft and a glazed lip. Another clue suggests that oil consumption is increasing. Repair small leaks promptly so they don't cause damage.

prev
O-Ring Design, Surface Quality, and Installation: A Complete Guide to Reliable Sealing
How to Select the Best Lip Seal Manufacturer for Industrial Applications
next
recommended for you
Get in touch with us

Professional O Ring Suppliers &  O Ring Manufacturers

CONTACT US

TEL: +86-757-86235767

Contact Person: Teresa Chen

E-mail: dms@dmsseals.com

WhatsApp:13927708667

Mobile:13927708667

PAY ATTENTION TO US

Copyright © 2018 Fo shan Dms Seals Technology Co.,limited.  |  Privacy Policy  | Sitemap
Customer service